Damaged Paver Edging
Damaged Paver Edging is a moderate-severity finishes defect SURE inspectors have documented across 13 inspection reports.
Causes
- Not specified, common causes can include shrinkage stress, stress due to trees, commercial or heavy vehicle traffic, or soil movement due to changes in moisture content.
- Lack of proper sub-base or restraint
- Likely mechanical impact
- Lack of maintenance
- Poor installation
Symptoms to look for
- Visible damage or absence of edging/haunching
- Visible damage to a section of brick paving.
- Visible damage to paved driveway edging
- Visibly damaged or broken paver edging
- Damaged bricks in paved driveway
Remedies
- Engage a paving contractor for repairs to fix spreading pavers and damaged edging
- Rectification by the builder as per building standards.
- Engage a handyman/maintenance contractor for repairs
- Repair or replace damaged paver edging
- Realign/repair paver edging
Worth asking our inspector about this specifically.
This is common across Perth stock and usually fixable without drama, but the scope of the fix varies. Every SURE inspection includes 12 months of free advice. Call out the defect by name and we check for it directly.
Curated entries in Finishes
- Curated 1–3/5Common Cracks and Settlement in Pathways
Cracking and uneven settlement in concrete footpaths, driveways, and porch slabs is one of the most frequently observed external defects in Perth homes, present in 11.66% of all reports. Most findings are minor and reflect the expected behaviour of unreinforced concrete slabs on reactive soils, though tree-root intrusion and poor drainage can accelerate movement to a point where trip hazards develop.
- Curated 1–4/5Surface Rust on Pergola Frame
Surface oxidation on steel pergola frames is one of the more frequent cosmetic findings in Perth pre-purchase reports, appearing in 11.19% of all inspections. Left untreated, surface rust progresses through the coating into the base metal, eventually compromising the structural integrity of posts and beams. Early intervention with surface treatment is straightforward; through-corrosion is not.
- Curated 2–4/5Cracked Floor Tiles in Wet Areas
Cracked, loose, or drummy floor tiles in bathrooms, laundries, and kitchens. Allows moisture penetration to the substrate, potentially compromising waterproof membrane integrity and causing concealed water damage.
- Curated 1–3/5Damaged Eave Lining
Damage to the underside lining of the eaves - including cracking, holes, gaps at junctions, and poorly cut penetrations around downpipes - is recorded in 8.78% of all inspection reports. Beyond the cosmetic concern, openings in eave lining allow birds, possums, and insects to access the roof cavity and can accelerate timber deterioration where moisture also enters.
- Curated 1–3/5Eave Deterioration and Ageing
General weathering and paint breakdown on eave linings, timber rafter ends, and quad trim is one of the most common findings on Perth homes built before 2000. Left unattended, deteriorated eaves allow moisture into the roof perimeter, accelerating rot in rafter ends and creating conducive conditions for timber pests.
- Curated 1–3/5Defective Door Handles, Hinges, and Locks
Malfunctioning or worn door hardware including loose handles, squeaking hinges, misaligned latches, and non-functioning locks. High-frequency defect across all building eras, typically cosmetic but can affect security and fire egress.